Zircar Refractory Composites ALUMINA-SILICA MOLDABLE RS-C
Subcategory: Oxide, Silicon; Oxide, Aluminum; Oxide
Material Notes: ZIRCAR Alumina-Silica Insulating Blanket Type RS-C Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped rolled up and sealed in a plastic bag to preserve its moldability.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Compressive Strength
- Thermal Conductivity at Elevated Temperature
- Maximum Service Temperature, Air
- Shrinkage
- Color
|
|
|
|