Zircar Refractory Composites REFRACTORY SHEET RSLE-57
Material Notes: ZIRCAR Refractory Sheet Type RSLE-57 is a low expansion high strength reinforced silica matrix composite . This remarkable material was designed for use as a high strength insulator in induction hot press applications w. RSLE-57`s very low thermal expansion coefficient and high hot strength combine to give it thermal shock resistance not found in other structural ceramic matrix composite materials.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
| Available Properties |
- Density
- Porosity
- Hardness, Shore D
- Modulus of Rupture
- Compressive Strength
- Charpy Impact
- Volume Resistivity
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity at Elevated Temperature
- Shrinkage
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|