Zircar Refractory Composites REFRACTORY SHEET RSLE-501 CYLINDERS
Material Notes: ZIRCAR Refractory Sheet Type RSLE-501 is a low expansion high strength reinforced silica matrix composites in a cylindrical form. This remarkable material was designed for use as a high strength, durable insulator in induction heat treating applications. RSLE-501`s very low thermal expansion coefficient and high hot strength combine to give it thermal shock resistance not found in other structural ceramic materials.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
| Available Properties |
- Density
- Porosity
- Hardness, Shore D
- Modulus of Rupture
- Compressive Strength
- Charpy Impact
- Volume Resistivity
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity at Elevated Temperature
- Shrinkage
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|