Zircar Refractory Composites REFRACTORY SHEET RS-100
Subcategory: Oxide, Aluminum; Oxide
Material Notes: ZIRCAR Refractory Sheet Type RS-100 is a ceramic fiber reinforced structural alumina composite material with useful properties to 1260°C (2300°F). It has exceptional flexural and compressive strengths in the range of high temperature reinforced plastics such as G-7 and G-10 laminates and retains strength and utility to levels far exceeding maximum use temperatures of plastics. Mechanical properties of Type RS-100 sheet far exceed those of Transite TM and other asbestos-cement materials and is an excellent replacement for these rigid asbestos-containing products. Type RS-100 can also be employed at much higher temperatures than these types of products.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
| Available Properties |
- Density
- Loss On Ignition
- Porosity
- Hardness, Shore D
- Modulus of Rupture
- Compressive Strength
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Dielectric Breakdown
- Arc Resistance
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Maximum Service Temperature, Air
- Flammability Test
- Shrinkage
- Moisture Content
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|