Zircar Refractory Composites REFRACTORY SHEET RS-201

 

Subcategory: Oxide, Aluminum; Oxide

Material Notes:
ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivity and excellent electrical insulation. It retains strength and utility to levels far exceeding maximum use temperatures of reinforced plastics and asbestos cement replacements. It is 100% inorganic, non-flammable and contains no asbestos. Its high alumina content makes it resistant to many environments including molten aluminum. RS-201 undergoes little or no outgassing on heating, is not brittle, and may be cut and machined with standard tooling. RS-201 has a highly burnished outside surface. This is ideal when the OD is crucial for liner placement. It is available in standard and custom size cylinders and are useful as induction coil liners, induction furnace components, and molten metal transport tubes.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Available Properties
  • Density
  • Porosity
  • Modulus of Rupture
  • Compressive Strength
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Strength
  • Arc Resistance
  • CTE, linear 20°C
  • Thermal Conductivity at Elevated Temperature
  • Melting Point
  • Maximum Service Temperature, Air
  • Shrinkage
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。