Zircar Refractory Composites REFRACTORY SHEET RS-99R
Subcategory: Oxide, Aluminum; Oxide
Material Notes: Type RS-99R boards are prefired and are unaffected by moisture. They stay rigid even if saturated with water.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
| Available Properties |
- Density
- Loss On Ignition
- Porosity
- Specific Surface Area
- Modulus of Rupture
- Compressive Strength
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Shrinkage
- Color
|
|
|
|