Zircar Refractory Composites REFRACTORY SHEET RS-1200
Subcategory: Oxide, Aluminum; Oxide
Material Notes: ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-1200 is a combination of strong reinforcing fibers tightly bound in an alumina ceramic matrix. RS-1200 is completely inorganic and contains no asbestos or RCF fibers. RS-1200 exhibits greater refractoriness and homogeneity than other reinforced alumina matrix composite products and can be readily machined to tight tolerances with conventional carbide tooling.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
| Available Properties |
- Density
- Loss On Ignition
- Porosity
- Hardness, Shore D
- Modulus of Rupture
- Compressive Strength
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Dielectric Breakdown
- Arc Resistance
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Maximum Service Temperature, Air
- Flammability Test
- Shrinkage
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|