Zircar Refractory Composites REFRACTORY SHEET RS-99-45

 

Subcategory: Oxide, Aluminum; Oxide

Material Notes:
ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorganic binders. Type RS-99-45 has a high purity alumina bond making it well suited for use in high vacuum and reducing environments where silica cannot be tolerated, such as power metal and MIM furnaces with H2 atmospheres. It also has high electrical resistivity at elevated temperatures allowing it to be used in direct contact with resistance heating elements. It exhibits superior hot strength and dimensional stability to 1650°C (3000°F).

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Available Properties
  • Density
  • Porosity
  • Modulus of Rupture
  • Compressive Strength
  • CTE, linear 20°C
  • Thermal Conductivity at Elevated Temperature
  • Maximum Service Temperature, Air
  • Shrinkage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。