Zircar Refractory Composites REFRACTORY SHEET RS-A
Subcategory: Oxide, Aluminum; Oxide
Material Notes: ZRCI`s Refractory Sheet Type RS-A Moldable is a tough ceramic fiber reinforced insulation which contains no asbestos. Developed as an asbestos board replacement for induction coil liners and molten metal transport, Refractory Sheet Type RS-A Moldable is ideally suited for a wide range of high temperature, high thermal shock applications. Refractory Sheet Type RS-A Moldable is a wet blanket that can be easily formed into a wide variety of simple and complex shapes. Drying results in a strong rigid shape that can be rewet to restore the original moldability. Baking irreversibly removes the moldability, leaving Refractory Sheet Type RS-A Moldable unaffected by moisture. Refractory Sheet Type RS-A Moldable can be frozen and thawed repeatedly with no loss in moldability or other properties. Refractory Sheet Type RS-A Moldable can be dried rapidly, either with a torch or by applying directly to a hot furnace, to make quick repairs of cracks in, or to replace missing, refractories.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
| Available Properties |
- Density
- Solids Content
- Porosity
- Modulus of Rupture
- Compressive Strength
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|