Zircar Refractory Composites ALUMINA MAT RSMAT-3000

 

Subcategory: Oxide, Aluminum; Oxide

Material Notes:
ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot and has a higher alumina content than any other ceramic fiber mat or blanket. Type RSMAT-3000 is lightweight, has low thermal conductivity and low heat capacity, and is immune to thermal shock. It is ideal for vacuum, reducing atmospheres and other applications where silica cannot be tolerated, such as powder metal sintering, stainless steel bright annealing and many fuel cell applications.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Available Properties
  • Bulk Density
  • Loss On Ignition
  • Filament Diameter
  • Thickness
  • Ionic Impurities - Na (Sodium)
  • Hardness, Mohs
  • Tensile Strength, Ultimate
  • Modulus of Elasticity
  • Specific Heat Capacity
  • Thermal Conductivity at Elevated Temperature
  • Melting Point
  • Maximum Service Temperature, Air
  • Shrinkage
  • Calcium, ppm
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。