Zircar Refractory Composites ZIRCONIA COATING RS-ZIRGUARD

 

Subcategory: Oxide, Zirconium; Oxide

Material Notes:
ZRCI Zirconium Oxide Coating Type RS-ZIRGUARD is a cream colored, water based paint of Zirconium Oxide (ZrO2). It is produced using high-purity, partially stabilized Zirconium Oxide (4 wt% CaO). It provides a high purity ceramic coating with utility to 1900°C (3452°F). It exhibits high chemical resistance and excellent release properties. Type RS-ZIRGUARD produces a hard, abrasion and chemical resistant coating that protects all ceramic bodies against most molten metals and corrosive environments, protecting them from spalling, dusting, and chemical attack. Type RS-ZIRGUARD may be applied to soft or fibrous structures to produce a more wear resistant surface layer which is also resistant to most high temperature reactions which may degrade the ceramic.

Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)

Available Properties
  • Maximum Service Temperature, Air
  • Shelf Life
  • Color
  • Coverage, ft2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。