Copper Arsenic Sulfide, Cu3AsS4 (Enargite)
Subcategory: Sulfide/Chalcogenide; Semiconductor
Key Words: Chalcogenide; Semiconductor
Material Notes: Tetrahedral coordination in wurtzite superstructure. Luzonite is the zincblende-related mineral form of Cu3AsS4.
| Available Properties |
- Density
- a Lattice Constant
- c Lattice Constant
- Magnetic Susceptibility
- Band Gap
- CTE, linear 20°C
- Thermal Conductivity
- Heat of Formation
|
|
|
|