Copper Germanium Sulfide, Cu2GeS3, High Temperature Form
Subcategory: Sulfide/Chalcogenide; Semiconductor
Key Words: Chalcogenide; Semiconductor
Material Notes: Tetrahedral Coordination.
| Available Properties |
- Density
- a Lattice Constant
- Knoop Microhardness
- Magnetic Susceptibility
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Debye Temperature
|
|
|
|
| Property Data |