Zinc Telluride, ZnTe, Cubic
Subcategory: Sulfide/Chalcogenide; Semiconductor
Key Words: Chalcogenide; Semiconductor; Tellurium
| Available Properties |
- Density
- a Lattice Constant
- Knoop Microhardness
- Dielectric Constant
- Band Gap
- Electron Mobility, cm²/V-s
- Hole Mobility, cm²/V-s
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Heat of Formation
- Debye Temperature
- Refractive Index
- CAS Number
- Crystal Structure
|
|
|
|
| Property Data |