Chevron Phillips Shawinigan Black® Acetylene Black ABBEADW

 

Subcategory: Carbon

Key Words: Carbon, C

Material Notes:
SHAWINIGAN ACETYLENE BLACK is made from acetylene gas and is the purest form of carbon black available. Its unique structural properties offer high liquid absorption, high electrical conductivity, and the ability to impart this conductivity into plastics, rubber, and other materials. This product is in beaded form. It is free flowing, less dusty, and easier to handle than flake products.

Moisture: 0.10% Typical; 0.25% Max. Ash: 0.005% Max. Average bead hardness (16-18 mesh) is typically 7.0 g with a minimum value of 6.0 g. Mass strength is typically 100 psi with a minimum value of 20 psi. DBPA No is typically 204 cc/100 g with a minimum of 180 cc/100 g. AWSR (500 mesh seive) is typically 1.0 ppm with a maximum value of 4.0 ppm. pH is 7.0.

Data provided by Chevron Chemical.

Available Properties
  • Density
  • Apparent Bulk Density
  • Water Absorption
  • pH
  • Specific Surface Area
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。