Chevron Phillips Shawinigan Black® Acetylene Black AB50X GRIT
Subcategory: Carbon
Key Words: Carbon, C
Material Notes: SHAWINIGAN ACETYLENE BLACK is made from acetylene gas and is the purest form of carbon black available. Its unique structural properties offer high liquid absorption, high electrical conductivity, and the ability to impart this conductivity into plastics, rubber, and other materials. Moisture: 0.14% Typical; 0.2% Max. Ash: 0.29% Typical; 0.75% Max. Grit (325 Mesh Sieve): 0.007% Typical; 0.04% Max. Data provided by Chevron Phillips Chemical Company.
| Available Properties |
- Apparent Bulk Density
- Water Absorption
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|