Zoltek Panex® 33 48K Continuous PAN Carbon Fiber
Subcategory: Carbon Fiber; Carbon
Key Words: Carbon Fibres; Zoltek Corporation
Material Notes: Actual filament count is 45,700 Fiber Diameter 7.2 µm (0.283 mil) No twist 29,700 Denier (g/9000 m) 302 m/kg (450 ft/lb) yield 0.01825 cm² (0.00283 in²) average tow cross sectional area PANEX® continuous carbon fiber is manufactured from polyacrylonitrile (PAN) precursor. The consistency in yield and mechanical properties that are provided by the large filament count strands gives the user the ability to design and manufacture composite materials with greater confidence and allows for efficient and fast buildup of carbon fiber reinforced composite structures. Available with a variety of sizing formats for different composite processing methods and for compatibility with a wide range of standard sizing systems. Information provided by Zoltek Corporation.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Electrical Resistivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|