Zoltek Panex® 33 CF Chopped PAN Carbon Fiber
Subcategory: Carbon Fiber; Carbon
Key Words: Carbon Fibres; Zoltek Corporation
Material Notes: Fiber Diameter 7.2 µm (0.283 mil) PANEX® 33 CF chopped fibers are derived from Zoltek's high strength PANEX 33 carbon fibers. These are generally used for reinforcement in thermoplastic molding compounds requiring high strength and modulus, electrical conductivity, dimensional stability, low CTE, and excellent friction/wear properties. Can be provided either sized or unsized; electrical resistivity can also be modified. Information provided by Zoltek Corporation.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Electrical Resistivity
|
|
|
|