Hexcel® Carbon Fiber IM8 (12,000 Filaments)
Subcategory: Carbon Fiber; Carbon
Key Words: Carbon Fibres
Material Notes: Weight/length = 0.446 g/m. Information provided by Hexcel Corporation. Values are typical average lot properties. Continuous fiber can be combined with virtually all thermoset and thermoplastic resin systems. They are used for weaving, braiding, filament winding applications, unidirectional tapes and prepreg tow for fiber placement. Chopped fibers are used in compression and injection molding compounds to produce machine parts, gears, and chemical valves. The finished products have excellent corrosion, creep and fatigue resistance plus high strength and stiffness characteristics.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|