Antimony (III,V) Oxide, Sb2O4 (Cervantite)
Subcategory: Oxide, Other; Oxide
Key Words: Sb2O4
Material Notes: Yellow orthorhombic crystals
| Available Properties |
- Density
- Molecular Weight
- Hardness, Mohs
- CAS Number
- Color
- Crystal Structure
|
|
|
|
| Property Data |