Iron (II, III) Oxide, Fe3O4 (Magnetite)
Subcategory: Oxide, Other; Oxide
Key Words: Fe3O4
Material Notes: Black cubic crystals or amorphous powder. Weathering end product(s): Limonite, ochre. Occurrence: Igneous rocks, metamorphic. Weathers very slowly to limonite. Property values are typical of naturally occurring Magnetite (Fe3O4). Actual property values will vary from sample to sample.
| Available Properties |
- Density
- a Lattice Constant
- Formula Units/Cell (Z)
- Molecular Weight
- Hardness, Mohs
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 500°C
- Melting Point
- Refractive Index
- CAS Number
- Color
- Crystal Structure
|
|
|
|