Iron (III) Oxide, Fe2O3 (Hematite)
Subcategory: Oxide, Other; Oxide
Key Words: Fe2O3
Material Notes: Red-brown hexagonal crystals. Weathering end product(s): Limonite, ochre. Occurrence: Pigment in sediments. Hydrates slowly to limonite, rust burst. Property values are typical of naturally occurring Hematite (Fe2O3). Actual property values will vary from sample to sample.
| Available Properties |
- Density
- a Lattice Constant
- Beta Lattice Angle
- Formula Units/Cell (Z)
- Molecular Weight
- Hardness, Mohs
- CTE, linear 20°C
- CTE, linear 500°C
- Melting Point
- Refractive Index
- CAS Number
- Color
- Crystal Structure
|
|
|
|
| Property Data |