Molybdenum (IV) Sulfide, MoS2 (Molybdenite)
Subcategory: Sulfide/Chalcogenide
Key Words: MoS2
Material Notes: Black powder or hexagonal crystals
| Available Properties |
- Density
- a Lattice Constant
- b Lattice Constant
- Formula Units/Cell (Z)
- Molecular Weight
- Hardness, Mohs
- Melting Point
- CAS Number
- Color
- Crystal Structure
|
|
|
|