Nitrogen Selenide, N4Se4
Subcategory: Sulfide/Chalcogenide
Key Words: N4Se4
Material Notes: Red monoclinic crystals, hygroscopic
| Available Properties |
- Density
- Molecular Weight
- Color
- Crystal Structure
|
|
|
|