American Elements Barium Titanate nanoparticles
Key Words: Formula: BaTiO3; CAS Number: 12047-27-7
Material Notes: General DescriptionBarium Titanate Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nanoscale Barium Titanate Particles are typically 20-40 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range and also available in with an average particle size of 100 nm range with a specific surface area of approximately 7 m 2 /g. Nano Barium Titanate Particles are also available in ultra high purity and high purity and coated and dispersed forms. Applications for Barium Titanate Nanocrystals include for their dielectric properities and in the capacitors for microelectronics and future nano-electronics.
| Available Properties |
- Particle Size
- Specific Surface Area
- Molecular Weight
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|