American Elements Lithium Manganese Dioxide Nanoparticles
Key Words: Formula: LiMnO2; CAS Number: 7439-93-2/1313-13-9
Material Notes: General DescriptionLithium Manganese Oxide (LiMnO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Lithium Manganese Oxide Particles are typically 10 - 50 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range. Nano Lithium Manganese Oxide Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Research into applications for lithium manganese oxide nanocrystals has focused on developing lower-cost cell component materials, such as coated or treated natural graphites for battery anodes, in a composite cathode for rechargeable lithium batteries to both accelerate charge and discharge time as well as for their other potential electrical, dielectric, magnetic, optical, catalytic, biomedical and bioscience properties and for use in coatings, plastics, nanowire, nanofiber and textiles and in alloy and catalyst applications.
| Available Properties |
- Particle Size
- Specific Surface Area
- Appearance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|