American Elements Nickel Nanoparticles

 

Subcategory: Pure Element; Nonferrous Metal

Key Words: Formula: Ni; CAS Number: 7440-02-0

Material Notes:
General Description

Nickel (Ni) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Nickel Particles are typically 10 - 40 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range and also available in with an average particle size of 50 - 100 nm range with a specific surface area of approximately 5 - 10 m 2 /g. Nano Nickel Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Applications for nickel nanocrystals include numerous catalytic functions such as in the anode of solid oxide fuel cells (SOFC) or in the conductive electrolytic layer of proton exchange membrane (PEM) fuel cells, in replacement of platinum. Also, substituting all or a portion of the platinum with nickel nano particles in automotive catalytic converters would significantly reduce their cost and in coatings, plastics, nanowire, nanofiber and textiles and in certain alloy and catalyst applications. Further research is being done for their potential electrical, dielectric, magnetic, optical, imaging, biomedical and bioscience properties.

Available Properties
  • Particle Size
  • Specific Surface Area
  • Molecular Weight
  • Appearance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。