American Elements Niobium Nanoparticles
Subcategory: Pure Element; Nonferrous Metal
Key Words: Formula: Nb; CAS Number: 7440-03-1
Material Notes: General DescriptionNiobium (Nb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Niobium Particles are typically 10-20 nanometers (nm) with specific surface area (SSA) in the 30 – 60 m 2 /g range and also available in with an average particle size of 80 nm range with a specific surface area of approximately 12 m 2 /g. Nano Niobium Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Niobium nanocrystals include as electrocatalysts and as a superconductor and further research is being done for their Anisotropic Thermal Conductivity electrical and dielectric properties.
| Available Properties |
- Particle Size
- Specific Surface Area
- Molecular Weight
- Appearance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|