American Elements Platinum Nanoparticles
Subcategory: Pure Element; Nonferrous Metal
Key Words: Formula: Pt; CAS Number: 7440-06-4
Material Notes: General DescriptionPlatinum (Pt) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Platinum Particles are typically 20 - 100 nanometers (nm) with specific surface area (SSA) in the 1 – 3 m 2 /g range. Nano Platinum Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Platinum nanocrystals include numerous uses in catalysts (including catalytic converters), electrocatalysts, chemical synthesis (also in silver-platinum nanoparticles) and as a Magnetic Nanopowder (also in iron-platinum nanoparticles) and deposed on silica and carbon nanotubes, in polymer membranes to create Active Polymer Membranes for Proton Exchange Membrane (PEM) fuel cells and in other coatings, plastics, nanofiber and textiles and in nanowire and other catalysis applications.
| Available Properties |
- Particle Size
- Specific Surface Area
- Molecular Weight
- Appearance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|