American Elements Tantalum Oxide Nanopowder
Subcategory: Oxide, Other; Oxide
Key Words: Formula: Ta2O5; CAS Number: 1314-61-0
Material Notes: General DescriptionTantalum Oxide ( TaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tantalum Oxide Particles are typically 20-80 nanometers (nm) with specific surface area (SSA) in the 10 – 50 m 2 /g range and also available in with an average particle size of 100 nm range with a specific surface area of approximately 7- 10 m 2 /g. Nano Tantalum Oxide Particles are also available in ultra high purity and high purity, transparent, and coated and dispersed forms. Applications for Tungsten Oxide Nanocrystals include in dental imaging because they are sufficiently radiopaque (is impervious to radiation) for good X-ray resolution, and in coatings, plastics, nanowire, nanofiber and textiles and in certain alloy and catalyst applications. Further research is being done for their potential electrical, dielectric, magnetic, optical, imaging, biomedical and bioscience properties.
| Available Properties |
- Particle Size
- Specific Surface Area
- Molecular Weight
- Appearance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|