American Elements Tin Nanoparticles
Subcategory: Pure Element; Nonferrous Metal
Key Words: Formula: Sn; CAS Number: 7440-31-5
Material Notes: General DescriptionTin (Sn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tin Particles are typically 10-20 nanometers (nm) with specific surface area (SSA) in the 30 – 60 m 2 /g range and also available in with an average particle size of 80 nm range with a specific surface area of approximately 12 m 2 /g. Nano Tin Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Tin nanocrystals include in transparent ant-static film, as an anti-microbial, anti-biotic and anti-fungal agent when doped with silver and incorporated in coatings, plastics, nanofiber, bandages and textiles. Further research is being done for their potential as confined acoustic and optic phonons and for their electrical, biomedical and bioscience properties. Tin Nano Particles are generally immediately available in most volumes.
| Available Properties |
- Density
- Particle Size
- Specific Surface Area
- Molecular Weight
- Melting Point
- Boiling Point
- Appearance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|