Old Hickory Clay Co. Ultra Cast 33 Slurry
Subcategory: Clay; Slurry
Key Words: ball clays, slurries
Material Notes: Warning: Ball clays contain free silica. Do not breathe dust. Prolonged inhalation may cause delayed lung injury (silicosis). Follow OSHA Safety and Health Standards for Crystalline Silica (Quartz). For further information consult the Old Hickory MSDS for this clay. Data provided by the manufacturer, Old Hickory Clay Company.
| Available Properties |
- Loss On Ignition
- Particle Size
- Soluble Sulfates
- Specific Surface Area
- Modulus of Rupture
|
|
|
|
| Property Data |