Old Hickory Clay Co. Clay 760-C Slurry
Subcategory: Clay; Slurry
Key Words: ball clays, slurries
Material Notes: Clean, kaolinitic, ball clay slurry blend for use in filler applications, ceramic tile body and glaze applications. High purity and excellent suspension properties are trademarks of the product. Data provided by the manufacturer, Old Hickory Clay Company.
| Available Properties |
- Loss On Ignition
- Particle Size
- pH
- Soluble Sulfates
|
|
|
|