Omya OMYACARB® FT - FL Calcium Carbonate
Subcategory: Additive/Filler for Polymer
Material Notes: A high purity, fine, wet ground, surface-treated natural calcium carbonate. Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such as water based, solvent based, and high gloss powder coatings. Information supplied by Omya North America.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Particle Size
- Specific Surface Area
- Refractive Index
- Reflection Coefficient, Visible (0-1)
- Calcium Carbonate %
- FDA
- Hegman (dry)
- Magnesium Carbonate %
- Percent Finer than 1 Microns
- Percent Finer than 2 Microns
- Pounds Pigment/Solid Gallon (dry)
- Retained in 325 mesh (dry) ppm
- Treatment %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|