Omya OMYACARB® 3 - FL Calcium Carbonate
Subcategory: Additive/Filler for Polymer; Slurry
Material Notes: A beneficiated calcium carbonate with excellent fineness, color, and dispersion characteristics available in dry and slurry forms. Applications: Employed in rubber and plastic applications such as rigid PVC and plasticized PVC. Also used in all types of coatings and paints, putties, caulk, and sealants. Information supplied by Omya North America.
| Available Properties |
- Specific Gravity
- Density
- Solids Content
- Moisture Absorption at Equilibrium
- Particle Size
- Specific Surface Area
- Refractive Index
- Reflection Coefficient, Visible (0-1)
- Calcium Carbonate %
- FDA
- Hegman (dry)
- Magnesium Carbonate %
- Pounds Pigment/gallon (slurry)
- Pounds Pigment/Solid Gallon (dry)
- Retained in 325 mesh (dry) ppm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|