Omya OMYACARB® BP - LU Calcium Carbonate
Subcategory: Additive/Filler for Polymer
Material Notes: An intermediate, dry ground calcium carbonate with a closely controlled particle size distribution. Applications: A de-dusted filler that is ideal for joint compounds, unsaturated polyester, cementitious grouts, plasters, paints, plastics, and adhesives. Information supplied by Omya North America.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Particle Size
- Reflection Coefficient, Visible (0-1)
- Calcium Carbonate %
- FDA
- Magnesium Carbonate %
- Retained in 325 mesh (dry), %
|
|
|
|