Omya OMYACARB® 10 - AZ Calcium Carbonate
Subcategory: Additive/Filler for Polymer
Material Notes: A dry ground calcium carbonate with an intermediate and closely sized particle distribution. Applications: Am ideal extender for plastics, rubber, coating, and caulks. Designed for use in unsaturated polyester compounds (BMC, SMC). Also used in paint applications, sealants, and adhesives. Information supplied by Omya North America.