Omya OMYACARB® 2 - LU Calcium Carbonate
Subcategory: Additive/Filler for Polymer
Material Notes: A fine, dry ground calcium carbonate with excellent color and dispersion characteristics. Applications: Plastic applications such as rigid PVC, flexible PVC, and polyolefins. Paint applications such as water based, solvent based, and high gloss powder coatings. Information supplied by Omya North America.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Particle Size
- Reflection Coefficient, Visible (0-1)
- Calcium Carbonate %
- DOP Absorption, g DOP/100 g pigment
- FDA
- Hegman (dry)
- Magnesium Carbonate %
- Oil Absorption, g oil / 100 g pigment
- Retained in 325 mesh (dry) ppm
|
|
|
|