Omya OMYACARB® 3 - AZ Calcium Carbonate
Subcategory: Additive/Filler for Polymer
Material Notes: A dry ground calcium carbonate with excellent fineness, color, and dispersion characteristics. Applications: Rubber and plastic applications such as rigid and plasticized PVC. Also used in paints, putties, caulk, and sealants. Information supplied by Omya North America.
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Particle Size
- Reflection Coefficient, Visible (0-1)
- Calcium Carbonate %
- FDA
- Hegman (dry)
- Magnesium Carbonate %
- Retained in 325 mesh (dry) ppm
|
|
|
|