Omya CAL® USP-15 AZ Food Grade Calcium Carbonate
Material Notes: This product is made under strict quality control measures to insure that it meets the requirements of the U.S. Pharmacopeia and Food Chemicals Codex monographs for Calcium Carbonate. Information supplied by Omya North America.
| Available Properties |
- Moisture Absorption at Equilibrium
- Particle Size
- Acid Insoluble, %
- Calcium Carbonate %
- FDA
- Magnesium and Alkali Salts %
|
|
|
|