Poco Graphite ZXF-5Q Specialty Graphite

 

Subcategory: Graphite; Carbon

Material Notes:
SSH hardness is 86.

General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small particle size allow fabrication of complex components containing tight tolerances. Post synthesis treatments available include purification or impregnation with resins, oxidation inhibitors, or metals. Surface treatments offer improved wear characteristics and particle reduction.

Some applications of Poco specialty graphites include anode plates for wet cells, fuel cell plates for solid polymer cells, air bearings, hot gas valves, high temperature bearings, bushings, and seals, hot press dies and rams, furnace furniture/fixturing, rocket engine nozzles, molten metal casting components, vacuum furnace heating elements, space vehicle nose cones, mirrors and optical structures, and satellite heat shields.

Information provided by Poco Graphite, Inc.

Available Properties
  • Density
  • Apparent Bulk Density
  • Open Porosity
  • Porosity
  • Particle Size
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Modulus of Elasticity
  • Flexural Strength
  • Compressive Yield Strength
  • Electrical Resistivity
  • CTE, linear 20°C
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。