Poco Graphite Durabraze® Purified/Machined Specialty Graphite
Subcategory: Graphite; Carbon
Material Notes: Shore scleroscope C-2 hardness is 77. DURABRAZE is the trade name for a high-strength, finished product that has been purified, machined and subjected to Poco Graphite's proprietary carbon modification treatment. DURABRAZE products are designed for use as fixturing devices for the glass to metal seal and brazing industries. They are ideal for applications requiring an abrasion-resistant, particle-free surface. The graphite substrate is a fine-grained, high strength graphite that has excellent machinability. The graphite is next purified and given a unique amorphous carbon treatment. This treatment is unique because it does more than coat the surface. It also infiltrates and locks onto the graphite. This treatment provides a hard, abrasion resistant surface that produces no particles. The result is a surface that is grain free, harder than the substrate, but extremely thin and uniform on all surfaces. This treatment does not affect the ability to maintain tight tolerances. Information provided by Poco Graphite, Inc.
| Available Properties |
- Density
- Apparent Bulk Density
- Tensile Strength, Ultimate
- Flexural Strength
- Compressive Yield Strength
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Maximum Service Temperature, Inert
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|