Silberline Sparkle Silver® 3333-AR
Subcategory: Ceramic/Metallic Coating
Material Notes: Sparkle Silver® 3333-AR is an acid resistant pigment developed for formulators requiring good face whiteness, with a fine appearance. Close packing and good distinctiveness of image (D.O.I.) make Sparkle Silver® 3333-AR a good choice for basecoat/clear automotive systems.Applications: Automotive
| Available Properties |
- Specific Gravity
- Bulk Factor
- Volatiles
- Particle Size
- Particle Mesh Size
- Solvents
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|