Silberline Sparkle Silver® 3641
Subcategory: Ceramic/Metallic Coating
Material Notes: Sparkle Silver® 3641 is a coarse, regular purity, non-leafing aluminum pigment. It is characterized by high sparkle, a white face color and deep flop. An acid resistant purity version, Sparkle Silver® 3141-ST, is also available.Applications: Automotive; General Industrial
| Available Properties |
- Specific Gravity
- Bulk Factor
- Volatiles
- Particle Size
- Particle Mesh Size
- Solvents
|
|
|
|