Silberline Sparkle Silver® 5745
Subcategory: Ceramic/Metallic Coating
Material Notes: Sparkle Silver® 5745 is a fine, regular purity, non-leafing aluminum pigment with good opacity for solvent-based general industrial coatings. It provides excellent distinctiveness of image (D.O.I.) and brightness.Applications: Automotive; General Industrial
| Available Properties |
- Specific Gravity
- Bulk Factor
- Volatiles
- Particle Size
- Particle Mesh Size
- Solvents
|
|
|
|