Silberline "A" Series A-2291FG
Subcategory: Ceramic/Metallic Coating
Key Words: ASTM D962-86 Type IV, Class A
Material Notes: A-2291FG is an ultra fine, high opacity, non-leafing aluminum pigment for solvent based general industrial coatings. Due to the small particle size, this grade is well suited for imparting high opacity at low loading levels. This grade is not recommended for use with chromatic pigments, as it will not produce clean coloristic effects.Applications: General Industrial
| Available Properties |
- Specific Gravity
- Bulk Factor
- Volatiles
- Particle Size
- Particle Mesh Size
- Solvents
|
|
|
|