Silberline EternaBrite® 601-PA

 

Subcategory: Ceramic/Metallic Coating

Material Notes:
EternaBrite® pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on cornflake geometry and offer enhanced leafing properties in solvent and waterborne flexographic and gravure inks for stronger metallic effects. Although EternaBrite® pigments can be used in aqueous inks they are not treated to protect against the aluminum-water reaction and special care must be taken to evaluate the gassing stability of each grade in the final ink formulation. High or excessive shear during ink production can initiate the aluminum-water reaction. Care must be taken to avoid excessive or high shear during processing when used in ink formulations containing water.

Applications: Printing Inks

Available Properties
  • Specific Gravity
  • Volatiles
  • Particle Size
  • Category
  • Solvents
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。