Silberline Standard Series A-6578FG
Subcategory: Ceramic/Metallic Coating
Key Words: ASTM D962-86 Type II, Class A; Fed. TT-P-320D Type II, Class A
Material Notes: A-6578FG is a standard polished grade; class A, fine leafing aluminum pigment carried in C-66 exempt mineral spirits.Applications: Trade & Maintenance
| Available Properties |
- Specific Gravity
- Bulk Factor
- Volatiles
- Particle Size
- Particle Mesh Size
- % Leaf (min)
- Solvents
- Water Coverage (cm²/gm)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|