Thornel® Carbon Fiber T-650/35 12K, Polyacrylonitrile (PAN) Precursor
Subcategory: Carbon Fiber; Carbon
Close Analogs: Thornel® products were sold by Amoco and are now owned by Cytec.
Key Words: Carbon Fibre; BP Amoco Performance Products, Inc.
Material Notes: Data provided by the manufacturer, Amoco Performance Products, Inc. Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated to increase the interlaminar shear strength in a resin matrix composite. 12000 filaments/strand, 94% carbon assay, 6.8 µm filament diameter, 1.31 m/g yield, 0 tpm twist (also available twisted), 0.432 mm² fiber area in yarn cross section.
| Available Properties |
- Density
- Specific Surface Area
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|