Thornel® Carbon Fiber P-25 2K, Pitch Precursor
Subcategory: Carbon Fiber; Carbon
Close Analogs: Thornel® products were sold by Amoco and are now owned by Cytec.
Key Words: Carbon Fibre; BP Amoco Performance Products, Inc.
Material Notes: Data provided by the manufacturer, Amoco Performance Products, Inc. Continuous filament strand from a pitch precursor. 2000 filaments/strand, 97+% carbon assay, 11 µm filament diameter, 3.1 m/g yield, 0 tpm twist, 0.17 mm² fiber area in yarn cross section.
| Available Properties |
- Density
- Specific Surface Area
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- Thermal Conductivity
|
|
|
|